The copper sulfate idea is appealing and I may give it a try.
This morning I just went up on the roof (before the blistering heat
that's forecast) and scraped off the patches of lichen and tarred the
scraped places. That will reduce the chance of breaches in the
shingles.
I wonder whether lichen always could grow on asphalt shingles, or if
this is some evolutionary development.
On Sat, Jul 3, 2010 at 5:40 PM, Peter Fels & Phoebe Palmer
<artgawk at thegrid.net> wrote:
> LOL...I heard to mix them with dilute milk but i like
> your version better Jerry.
>
> Jerry Frost wrote:
>> Oh yeah, one last thing. Alcohol will have zero effect on lichen except
>> maybe make it happier and grow better. Whatever you do do NOT let anyone
>> getting on the roof take a beer. The sure fire fast track method of
>> propogating lichen is to drop some in a blender with a boch beer dilute the
>> results 50/50 with water and spray it on whatever you want lichen on.
>> Decorative boulders and such being most common. Water it a couple times a
>> week or so and stand back, the sprayed area will have healthy fast growing
>> colonies of lichen established in days, weeks if you live in a DRY climate
>> but still.
>>
>> So anywho, spraying your roof with alcohol and scrubbing with a brush will
>> only serve to spread the lichen everywhere the brush touches which is just
>> the opposite I believe you want.
>>
>> Jer
>> -------------------------
>> If it ain't forged
>> It ain't real
>> wrought iron is
>> The Frostworks
>>
>>
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Bruce
NJ
More information about the TheForge
mailing list