[TheForge] brazing revisited

Woolley wjec1 at verizon.net
Fri Jan 29 21:27:40 EST 2010


Grover.Richardson at gtri.gatech.edu wrote:
>
> Another topic I thought of, instead of using splatter spray, I generally also just use cheap Home Depot flat black spray paint.  The splatter will "stick," but be loose enough due to the coating that it will come off very easily.  And I don't have to worry about getting the oil based anti-splatter coatings off.
>
>   


What do you use to remove the anti spatter, lacquer thinner?  I remember 
in the field one time some years ago we were installing a pretty large 
expansion joint on a stack at a power plant.  It was stainless and we 
had to do a lot of welding on it.  It was shaped like a bellows so there 
was quite a bit of overhead welding which would have deposited a lot of 
small balls of spatter.  They bought some powdered mixture that had to 
be blended with water.  It was the consistency of light pan cake batter 
that we brushed on.  When it dried we did all the welding and nothing 
stuck to it.   I never saw it again but might be worth lookin up.