Yes, some folks I know have used PAM because it is cheaper and appears to work "good enough<G>."

-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Peter Fels & Phoebe Palmer
Sent: Friday, January 29, 2010 6:13 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] brazing revisited

Hi Grover..Pam cooking spray is supposed to work for spatter too..but it 
is oil.  pf

Grover.Richardson at gtri.gatech.edu wrote:
> Understood.  I tend to do the low tech stuff also, but I happened upon this, and my mind flashed, so figured to share.
> 
> Another topic I thought of, instead of using splatter spray, I generally also just use cheap Home Depot flat black spray paint.  The splatter will "stick," but be loose enough due to the coating that it will come off very easily.  And I don't have to worry about getting the oil based anti-splatter coatings off.
> 
> All the best.
> 
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Peter Fels & Phoebe Palmer
> Sent: Thursday, January 28, 2010 1:27 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] brazing revisited
> 
> Hi Grover;
> Couldn't find a listing for the wet rags i generally use instead.
> My 25 year old tube of heat-stop is still unopened on the shelf.
> PS..skip using synthetic rags for this.
> 
> Grover.Richardson at gtri.gatech.edu wrote:
>> Lenox Sterling(r) ColdCoat(r) Thermal Shield Paste 32 oz. WS80326 1UYK4 36.60
>> Markal Cool Gel Heat Barrier Spray 16 oz. 83495G 2AGV8 13.92
>> Cool Blue(tm) Heat Sink Paste 11 oz. 91861 5KH10 11.48
>>
>> Just found this.
>> >From Grainger.com
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html


More information about the TheForge mailing list