On 12/21/2010 9:48 AM, Andrew Vida wrote:
>
> xlch58 at swbell.net wrote:
>> Cut them real thin and stack them and glue them around the rim of the
>> plywood. No steaming necessary.
> The plywood acts as the caul. Needs a lot of clamps for that come off
> well where concavity in the strips occurs unless you use a separate caul
> to distribute the clamping force evenly - a good idea in any case.
I just wrap it with haybaling twine and pull it tight as I go when I
need to go this way. This is the way Luthiers do it.