[TheForge] Power hammers

peter fels & phoebe palmer artgawk at thegrid.net
Mon Dec 20 17:26:35 EST 2010



On 12/20/2010 1:06 PM, Andrew Vida wrote:
>
> Kim George wrote:
>> What ever happened to the self contained hammer that was made in
>> Turkey? The quality was good as I remember. None of this tear it down
>> and rework it out of the crate.
> Sahinler.  All I remember was at the 98 Conference the one they fired up
> started smoking in under 5 minutes and went tits-up.  The German hammer
> worked all day without a hiccup.  Draw from that what you may.
Think Mark K said there were over long rubber hoses in it that 
overheated and fried. Shouldn't have been rubber at all.
Wasn't that the conf ( i missed it) that Mark won the junk yard hammer 
contest with his self contained JYH?
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>