Mine's a wine barrrel cut in half. It actually froze two weeks ago, and I 
emptied it.  I had to go to the dentist today, so I stopped in the farm 
store and got the heater.  I've never had ice break a barrel, but I always 
empty them as soon as the surface freezes.  Over the years I've had several 
plastic buckets freeze and break, if I leave them over the weekend and 
forgot to empty on Friday. One of the problems with emptying the barrel in 
the winter, is it dries out and I have to resoak it in the spring or it 
won't hold water. I know a guy that runs a cooperage, I asked him if they 
have to soak new barrels. He said no, they are tight enough when new to not 
leak. But after they have been used the wood shrinks and has to be soaked to 
swell up and seal. If they took used barrels back to the cooperage and 
tightened the bands with their big press, you may not have to soak, but that 
would be a lot of extra work.

Robert Ehrenberger
Shelbyville, Mo.
eforge at centurytel.net

----- Original Message ----- 
From: <williamsiron at comcast.net>
To: "Bob Ehrenberger" <eforge at centurytel.net>; "Blacksmithing List Sponsored 
by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, December 16, 2010 8:24 PM
Subject: Re: [TheForge] Slack tank




Bob,



While my shop gets cold enough to freeze water and then some, I just let my 
slack tub freeze. I've got a stainless steel former beer keg with the top 
cut out as a slack tub. Let me know how the heater works.



We've had unusually cold weather lately. 3 inches of snow today with low 
temps in the teens and wind chills in single digits. The shore usually has a 
milder climate.



Mark Williams

Snow Hill, Maryland
----- Original Message ----- 
From: "Bob Ehrenberger" <eforge at centurytel.net>
To: "theforge" <theforge at mailman.qth.net>
Sent: Thursday, December 16, 2010 7:22:52 PM
Subject: [TheForge] Slack tank

I finally broke down and got a tank heater for my half barrel. Usually this
time of the year I empty the barrel and work out of a 5 gal. bucket which I
would dump every couple days when it was cold. At the black friday
hammer-in I noticed our host had a tank heater, and asked if it was
expensive to run. He said that he could hardly tell the difference. I have
my shop on it's own meter so I'll have a pretty good idea if it is costing
me a lot more.

Robert Ehrenberger
Shelbyville, Mo.
eforge at centurytel.net


______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoworks.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html



-----
No virus found in this message.
Checked by AVG - www.avg.com
Version: 10.0.1170 / Virus Database: 426/3319 - Release Date: 12/16/10



More information about the TheForge mailing list