Somewhere I believe read something about a fusion layer that, IIRC, was
essentially a thin layer of thermite. Imagine taking a sheet of "paper",
cutting it to size, and placing it between anvil and steel plate. The fit
would have to be good -- IIRC, this stuff had no gap-filling ability. Set
it off, and instant weld.
Now, is this real or am I dreaming.
The IRD 100 awards, maybe 10-20 years ago, seems a likely place I might
have read such a thing. I'll check and may report back.
On Sun, Dec 12, 2010 at 9:58 AM, Andrew Vida <osan at netlabs.net> wrote:
> Just had a thought, so take cover.
>
> Has anyone ever tried welding a face using thermit? A think layer of
> thermit interposed between the wrought body and steel face, clamped
> elastically perhaps? Light bugger off and watch the fun!
>
>
>
> CGRAF wrote:
> > I seem to remember ( and Seeming to remember is happening more and more)
> > that some of the tool steel tops were welded to the base of cast anvils
> > by placing the heated steel plate in the mold and pouring the cast over
> it.
> >
> > It might work, but I cannot find any corroborating documents in my piles
> > of crap.
> >
> > At any rate it sounds less nasty than trying to forge weld a 3/4 inch
> > plate onto a base.
> >
> > Am I remembering something real or just a dream?
> >
> > Mike Graf
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is
> > http://www.photoaccess.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net
> > Please help support this email list: http://www.qsl.net/donate.html
> >
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Bruce
NJ
More information about the TheForge
mailing list