[TheForge] OT - rust-proof spring needed

John Allen countrymetals at gmail.com
Fri Aug 27 14:41:46 EDT 2010


I have made some big springs before with a pipe and blocking on my old Oster
pipe threader

On Aug 27, 2010 2:26 PM, "Paul" <forge at wi.rr.com> wrote:

On 8/27/2010 7:13 AM, barkingcrow at comcast.net wrote:
> What's involved in making a spring on your ...
Take a look here for more inspringation:

http://home.earthlink.net/~bazillion/setup.html

--
Paul
WB9HCO
My Grandfather WAS a blacksmith...
and it didn't do me one damn bit of good.
All opinions are the personal beliefs of the author, and are based on
decades of experience... so use your best judgement, I'm just a lowly
crafstman.
 "The difference between genius and stupidity is that genius has its
limits." -Albert Einstein
"Life is hard...it's harder if you're stupid" John Wayne - Sands of Iwo Jima