Very interesting thread- I was really excited about P-lac but it failed
badly when I used it on a couple of bright new expanded metal tabletops
(patio furniture).
Pete, more about why yours failed- was it the brushing, cuz I brushed mine.
Andy
--------------------------------------------------
From: "Lucky7Steel" <lucky7steel at gmail.com>
Sent: Sunday, August 08, 2010 8:15 PM
To: <theforge at mailman.qth.net>
Subject: Re: [TheForge] Chemicals- trials and tribulations
> Very interesting. thanks for all the info.
> Confusing though because isn't it an acid? If i don't rinse it off doesn't
> it just keep on ....blackening?
> I'll give a try just wiping then waxing though. I dont always have access
> to
> all the chemicals mentioned here because i live in Canada and i'm lucky to
> have figured out where to get the JAX i think! Can't get most things
> shipped
> dues to the Haz Mat status of a lot of these chemicals.
> On the chemicals side, has anyone tried Permalac spray laquer? I use
> Tremclad but i find it to suck mostly.
>
> ~Karen~
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list