Some alloys are slightly different but in general what you're looking
for is a black heat. It's just easier to heat it to cherry and let it
cool than trying to judge it in the fire. You should also quench it
about every third time. Re member when you do that you are annealing
the piece.All nonferrous metals are like that.

-- 