Take a heat the temp you want to weld at
Heat a piece of 1/16th steel to same color
Touch the two together they should stick if not not right temp
Roger R Degner
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of FireWorks PDX
Sent: Wednesday, August 04, 2010 2:20 AM
To: The Forge
Subject: [TheForge] Forge welding cable
I have a length of bright steel cable (1-1/2" diameter) that I want to forge
weld into a solid base for a sculpture. I'm using Z-weld flux. My first
attempt failed, I think due to a lack of heat, but I dunno. Maybe I'm not
getting flux in between the threads? Any advice? I'm going to check through
Zoeller's site, too, but I figured sending it out to y'all might help.
Thanks,
Mark
Fireworkspdx.com
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
****************************************************************************
********
This footnote confirms that this email message has been scanned by PineApp
Mail-SeCure for the presence of malicious code, vandals & computer viruses.
****************************************************************************
********
****************************************************************************
********
This footnote confirms that this email message has been scanned by PineApp
Mail-SeCure for the presence of malicious code, vandals & computer viruses.
****************************************************************************
********
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list