You are working it too hot. Heat it to cherry then wait until the
color leaves. You will have about 3 or 4 blows before it becomes to
hard to work. remember that when you start getting resistance to your
hit it's time to reheat and do it again.
On 8/4/10, Peter Fels & Phoebe Palmer <artgawk at thegrid.net> wrote:
> Anyone have an informal method of distinguishing between
> silicon bronze and architectural bronze ( with some lead
> in the alloy)?
> I have some bars of the stuff and it sure is willing to
> crack when it is worked hot...so i'm suspicious.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Kim George
"Why for you try to bury me in cold,cold ground?"
Taz
More information about the TheForge
mailing list