Whoa!
Fisher (a good brand) were guaranteed NOT to ring(shipyards& R.R.
yards).Only if the top is loose or half gone would it be considered "sunk".
I read "table" as the shelf instead of the anvil face. Therefore not
hardened (except Fisher), and repairable w/ mig wire. Free is good , but if
the face is destroyed, be patient till a good one comes along. Refinish
anvil face w/ MG750 rod ,if required. No pre/post heat req'd, and great for
diss-similar carbon content steels.
----- Original Message -----
From: "Peter Fels & Phoebe Palmer" <artgawk at thegrid.net>
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Saturday, April 24, 2010 3:37 AM
Subject: Re: [TheForge] Refurbishing an Anvil
> Garrick;
> If it thunks, then it's probably sunk.
> My suggestion is to use it like it is until you can pick
> up a good one.
> Use a 4" belt sander to take off the high spots.
> Refurbishing an anvil with a separated face plate is more
> work than it's worth. To do it well is expensive and very
> time consuming...Or you could forge weld the face back on
> and quench it with a fire hose.
>
> Garrick Peterson wrote:
>> I have access to an old anvil for a very reasonable price (i.e. free).
>> However, the anvil has seen quite a few years, and it's showing the
>> abuse.
>> The table is beat all to hell (defined as hammer marks creating nearly
>> 1/8"
>> ridges and valleys), and it has a very dull "thunk" when tapped with a
>> hammer.
>>
>> I'd like to make use of it, but I'm curious about what it would take to
>> refurbish the anvil, and whether it would be worth the time or cost.
>>
>> Thanks!
>>
>> -Garrick
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list