[TheForge] finish problem

Peter Fels & Phoebe Palmer artgawk at thegrid.net
Thu Apr 22 18:53:58 EDT 2010


Clyde:
I declare you master of the rust hustle!

Clyde wrote:
> I rust a lot of sculptures, some tiny, some 25 feet tall. I sold over 950
> last year plus many that I kept for my sculpture park, gave to schools etc.
> All are rusted so I need to rust a lot of stuff fast to keep up.
> 
>  
> 
> Peroxide alone is not good rust maker. A mixer of a pint of peroxide, a ¼
> cup of salt and a cup of 5% acid vinegar is a good start. If the iron is
> prepared right and the weather is warm and damp I can have a pretty passable
> rust in an hour. Overnight it looks great. 
> 
>  
> 
> You have to get the mill scale, dirt, paint, etc off. I use sandblasting or
> tumbling or a 10% solution of muriatic acid to get down to the bare metal.
> 
>  
> 
> After spraying on the mixture I rinse the piece off with a hose, sometimes
> after an hour, sometimes the next morning. It depends on the moisture in the
> air and temperature and the effect you want. 
> 
>  
> 
> Clyde Wynia
> 
> http://jurustic.com
> 
> http://flickr.com/photos/jurustic
> 
>  
> 
>  
> 
> I was trying to use peroxide to put a rust finish on some iron but it
> 
> did not work, what did I do wrong?  First cleaned in PH minus then
> 
> scrubbed with scotch brite pad under clean water got rid of excess
> 
> water and spray with peroxide.  Nothing happened, peroxide to week?
> 
> Allen
> 
>  
> 
>  
> 
> --
> 
> Allen Ortery
> 
> bluestoneforge at gmail.com
> 
> 309-368-7967
> 
> ______________________________________________________________
> 
>  
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 



More information about the TheForge mailing list