[TheForge] bandsaw steel problem
williamsiron at comcast.net
williamsiron at comcast.net
Tue Apr 6 20:50:43 EDT 2010
Andy,
Most bandsaw steel is L6.
Mark Williams
Snow Hill, Maryland
----- Original Message -----
From: "Andy Gladish" <gladish at cablerocket.com>
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, April 6, 2010 12:45:42 PM GMT -05:00 US/Canada Eastern
Subject: [TheForge] bandsaw steel problem
I'm looking for info on a steel problem:
Got my hands on a large steel cutting bandsaw blade from my local steel
supplier, one of the 1 1/2" wide ones.
I tried to "anneal" it by heating to nonmagnetic and throwing it on the
floor, but when I got to the part where you drill holes, it was no go even
with my gee whiz bits.
Any ideas on what steel it might be and/or how to soften it or get some
holes through the tang?
Thanks!
Andy G.
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list