[TheForge] bandsaw steel problem

Ron Childers munlaw2 at hcsmail.com
Tue Apr 6 14:02:32 EDT 2010


If a masonry bit won't do it, just put a rod in the drill press, kick it
wide open and burn it through.  

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Peter Fels & Phoebe
Palmer
Sent: Tuesday, April 06, 2010 1:16 PM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] bandsaw steel problem

Hi Andy:
Might be M2 or something fancy like that.
Perhaps taking it a bit above magnetic with a hefty chunk 
to steel strapped to it and bury it in ashes, lime or 
vermiculite to cool would work.

Andy Gladish wrote:
> I'm looking for info on a steel problem:
> Got my hands on a large steel cutting bandsaw blade from my local steel 
> supplier, one of the 1 1/2" wide ones.
> I tried to "anneal" it by heating to nonmagnetic and throwing it on the 
> floor, but when I got to the part where you drill holes, it was no go even

> with my gee whiz bits.
> Any ideas on what steel it might be and/or how to soften it or get some 
> holes through the tang?
> Thanks!
> Andy G. 
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html

 
 
****************************************************************************
********
This footnote confirms that this email message has been scanned by
PineApp Mail-SeCure for the presence of malicious code, vandals & computer
viruses.
****************************************************************************
********





 
 
************************************************************************************
This footnote confirms that this email message has been scanned by
PineApp Mail-SeCure for the presence of malicious code, vandals & computer viruses.
************************************************************************************





More information about the TheForge mailing list