[TheForge] Oxy/Propane reprise

Wayne Ackman stryker at vulcanpro.com
Fri Nov 6 20:05:18 EST 2009


thanks Peter and Ben:

glad to hear this will work.  I have the large Oxy bottle, but what 
about propane.   If I use the BBQ size, only cause they are everywhere.  
is there an issue connecting the hoses, now that they have some kind of 
weird new connector.

Or just thinking. maybe I should just tap into the line to my forge, 
that's a 250 gallon that provides for the whole shop, just need another 
split it and put in another shut-off.  Both options would be good tho'

Ben Barrett wrote:
> Wayne, I think you will be pleased.  I have a propane-specific gas
> saver, which is dandy,
> but a friend has a fuel saver built for acetylene which he uses on
> propane with no problems.
> I rigged up a simple foot-operated lever on the floor to switch my
> torch on when it is positioned in the vise (above and in-line with the
> pilot),
> and I got a cheap harbor freight torch which happens to be compatible
> with victor tips (I use a #0 and #2 propane-specific cutting tips,
> which were about $22 each at my local welding supply IIRC).  I did
> switch the hoses also, after multiple warnings that the cheaper hose
> made for acetylene will break down over time when exposed to propane,
> and develop slow leaks (hopefully they never spring for y'all who use
> the lesser grade!).  I have no trouble lighting the torch, but have
> not yet experimented with a brazing head (or a rosebud for that
> matter).
>
> The combination of a foot-controlled torch and a small fountain pump
> in my quench tank (supplying a stream of water above it) make quick
> and easy work of all sorts of small spot-heating and bending/shaping
> work.  There are times I want a jeweler-sized torch, and times I want
> much more heat, but I have been thinking I wished I had this torch
> setup before I even had a forge built!
>
> My only suggestion is to use the largest size oxy bottles you can
> handle, so you get a better price and don't have to swap them as
> often.  I'm curious about running a torch-like propane burner with
> forced air (compressor, hair dryer, etc) if it could maintain a flame
> in open air... anyone tried that sort of thing?  I know my propane
> forge can get hot enough to weld in, but I'm wondering what it takes
> to maintain a useful propane-air flame outside of the forge
> atmosphere/enclosure.  Just a matter of mixing the syrupy fuel with
> air, right?  Time to experiment some more, I suppose!
>
> Best wishes,
>
> Ben
>
>
> On Fri, Nov 6, 2009 at 4:58 PM, Peter Fels & Phoebe Palmer
> <artgawk at thegrid.net> wrote:
>   
>> Mine does.
>>
>> Wayne Ackman wrote:
>>     
>>> I have been thinking of getting a propane setup as the last job I did --
>>> curving the spiral on an oversize rail used a lot of gas.  But I was
>>> wondering,  if it is harder to light... will it work with a gas saver.
>>> I hang mine and it turns off.  and re-lights quickly as it passes the
>>> flame for the next use.  Will that work with propane?
>>>
>>>
>>> Ron Childers wrote:
>>>       
>>>> I bought a #2 propane adaptor tip for about $13 and it does a good job
>>>> heating or cutting railroad rail. The small Victor seems to work fine on
>>>> small stuff as-is. Trickier to light than acetylene....
>>>>
>>>>
>>>>
>>>>
>>>>
>>>>
>>>>
>>>>
>>>> ************************************************************************************
>>>> This footnote confirms that this email message has been scanned by
>>>> PineApp Mail-SeCure for the presence of malicious code, vandals & computer viruses.
>>>> ************************************************************************************
>>>>
>>>>
>>>>
>>>> ______________________________________________________________
>>>> TheForge mailing list
>>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>>> Help: http://mailman.qth.net/mmfaq.htm
>>>> Post: mailto:TheForge at mailman.qth.net
>>>>
>>>> TheForge mail list group photo site is
>>>> http://www.photoaccess.com
>>>> Login: blacksmithblacksmith at hotmail.com
>>>> Password: anvil
>>>>
>>>> This list hosted by: http://www.qsl.net
>>>> Please help support this email list: http://www.qsl.net/donate.html
>>>>
>>>>
>>>>         
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>>
>>> TheForge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>>
>>> This list hosted by: http://www.qsl.net
>>> Please help support this email list: http://www.qsl.net/donate.html
>>>
>>>       
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
>>     
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
>   


More information about the TheForge mailing list