>John, it would be interesting to know if they would still work following a
>temper at 212 F. Why 212 F - well that is a boiling water temper. We used
>to use that on some very very hard foil mill rolls. It would keep very high
>hardness but give some mesure of increased toughness. In that case the
>steel wasn't W1, but a alloy steel with 5 percent chrome.
>
>Dave
>
>--------------------------------------------------
>From: "John Switzer" <switz at mindspring.com>
>Sent: Tuesday, March 24, 2009 5:55 PM
>To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
>Subject: Re: [TheForge] flint strikers
>
> > I use new W1 and quench in brine with no temper. I have a very good
> > hot spark using a good sharp flint. If I temper I get nothing and if
> > I quench in plain water it seems to be hit and miss. These are
> > brittle hard, but I have rarely had a customer return one due to
> > breakage and I do guarantee them just because there is that chance.
> >
> >
> >
> >>I know we covered this before, but what was the consensus of opinion
> >>, to temper or use as quenched? From hay rake tines to files, seems
> >>they would be too brittle and hard to shave sparks in "as quenched".
> >>I expect it will be a "resultant" issue , as in, do two and see
> >>which showers best.
> >>
> >>
> >>dan tull
> >>Georgia
> >>______________________________________________________________
> >>TheForge mailing list
> >>Home: http://mailman.qth.net/mailman/listinfo/theforge
> >>Help: http://mailman.qth.net/mmfaq.htm
> >>Post: mailto:TheForge at mailman.qth.net
> >>
> >>TheForge mail list group photo site is
> >>http://www.photoaccess.com
> >>Login: blacksmithblacksmith at hotmail.com
> >>Password: anvil
> >>
> >>This list hosted by: http://www.qsl.net
> >>Please help support this email list: http://www.qsl.net/donate.html
> >
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is
> > http://www.photoaccess.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net
> > Please help support this email list: http://www.qsl.net/donate.html
> >
>______________________________________________________________
>TheForge mailing list
>Home: http://mailman.qth.net/mailman/listinfo/theforge
>Help: http://mailman.qth.net/mmfaq.htm
>Post: mailto:TheForge at mailman.qth.net
>
>TheForge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>Password: anvil
>
>This list hosted by: http://www.qsl.net
>Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list