[TheForge] Lathe dogs?

Bruce Freeman freemab222 at gmail.com
Mon Mar 16 13:26:00 EDT 2009


Larry,
I have the chucks, but some of the work I do may be center-to-center,
hence the need for the dogs.

Andy,
I have a small dog already, but would like larger sizes.  I'm going to
give a go at forging one tonight, time permitting.  I figure, wrap a
bar around a mandrel and weld the "tail."  I may rivet before welding,
welding in the rivet.  We'll see.



On Sun, Mar 15, 2009 at 10:06 AM, Andrew Vida <osan at netlabs.net> wrote:
> Given what you will be doing, a very small one will do.  I do have a
> small straight tail dog in my box if you want it.  It was part of my
> Schaublin setup.  You would have to make a driving lug for it, which
> would be a lot simpler than forging a dog.
>
> BTW, my machines will be coming home in a couple of weeks -  the
> Schaublin, Habbegers, Oliver, a new J-Head :).  Gotta put up a building.
>  Quickly.
>
>
> Bruce Freeman wrote:
>> I went to a swap meet and Englishtown flea market today, with no luck
>> finding lathe dogs.  Found a few other lathe tools, but passed up most
>> of them.
>>
>> I may try forging one on Monday.  Should be simple enough.
>>
>> On Sat, Mar 14, 2009 at 12:33 PM, Andrew Vida <osan at netlabs.net> wrote:
>>> Late on this note, but what else is new for me?
>>>
>>> Keep your eye open at Collingswood.  You may find one here or there.
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>>
>>> TheForge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>>
>>> This list hosted by: http://www.qsl.net
>>> Please help support this email list: http://www.qsl.net/donate.html
>>>
>>
>>
>>
>
> --
>
>     -Andy Vida
>
>             /\
>        __  /  \  __
>        \ \/ /\ \/ /   Proof Technologies Inc.
>         \ \/  \ \/    IV&V, Project and Program Management
>         /\_\__/\ \    Coming soon: parts for Star Reloaders
>        / ____/ /_ \   (304) 466-0789
>       /_/  \  /  \_\  osan at netlabs.net
>             \/
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>



-- 
Bruce
NJ

The total lack of evidence is the surest sign that the conspiracy is working.


More information about the TheForge mailing list