In reading that metalurgy book that was refered to on this forum which is
very good, almost a Blacksmithing Bible, It says when you burn charcoal it
produces either CO or CO2 depending on the temperature you burn it at, and
one of them (hot or cool) removes carbon from the steel and the other adds
it. Thats the jist of it anyway, my words it has diagrams too..
----- Original Message -----
From: "Daniel Kretchmar" <dan at irontreeworks.com>
>
> The article said that wootz can be made by cooking/baking cast iron
> for long periods (at very high temps) to burn out some of the carbon.
>