Daniel;
The sash weights i've seen were all cast iron...and funky cast iron at that.
They make very good sash weights...pf

Daniel Kretchmar wrote:
> I just received a sash weight as a gift.
> 
> Anybody know what they are made of?  It's pretty rusty. It looks like
> cast iron, but I suppose it could be wrought iron.
> 
> Danr