[TheForge] rusting
Mike Linn
bamablacksmith at comcast.net
Tue Mar 3 21:47:54 EST 2009
Muriatic isn't THAT toxic... just use a little common sense...
Another way .. heat the steel to 250-300deg F.. spritz with hydrogen
peroxide...
let sit in the sun...
repeat as necessary
mike
Lucky7Steel wrote:
> Anyone know a safer fairly quick way to rust steel other than using Muriatic
> acid? Too toxic for me i fear. Salt?
>
>
> ~Karen~