I have a love hate relationship with a very old Hobart handler


>For 1/4" ( i assume single pass) they list 700 IPM , 280 to 350 Amps,and
>31 to 34 Volts!...035 wire
>HONK! deposition rate is 11#/hr.
>That must leave me with a duty cycle time of about 12 seconds!.