Thanks Roger (and others)
I presently have been using the forge for "general" stuff, and only days
where I may have to put things away quickly (threat of rain) or if I
only have an hour or so available to me. But I prefer my smoky coal
beast, despite the having to move it.
But my "shop" is the area just outside my garden shed, so I have to move
things in and out. I just moved my canoe out of there, so I can at
least keep my vise and anvil "inside" for now. Maybe a new building
sometime soon.
Anyway, what I did when I made my forge was opt to NOT put a hinged door
on it (mistake #1), my (atmospheric) burners need to be closer together
to avoid a cold spot in between them. I''ll also add some sort of
door/gate that I can keep more heat INSIDE the forge. I fired it up
sunday ( 80 degree temps) and it was too much heat, too close to my
anvil. Even with the idler circuit, I had to take some breaks away from
it. (I'm still getting acquainted with using gas)
Also, I need to add choke plates to my burners, as I'm getting excessive
scale. I'm also not getting enough heat to forge weld, but that may just
be an indication that I need to keep more heat inside, or tune the
burners further.
I'm also wondering if maybe a 20lb bottle might be a better choice. I've
found that for somethings, the big bottle heats too much material, and I
end up quenching to do things like a bar end upset. Or better yet, I'll
keep the 30lb forge, and just move the burners between a small/larger
forge if I need a longer heat.
thx,
**paul
Roger Degner wrote:
> Can not help with the valve as the only ones I have removed are 100# ones.
> Some say to add dish soap to the water
>
> As for the forge are you building a knife forge or larger opening for
> general blacksmithing.
> This year at Batsons Knife symposium I watched Ken Swartzer make a Don
Fogg
> style upright knife forge.
>
> This only had two small openings to put the knife in and out the back if
> necessary. He said they once welded a long length of cable by putting the
> forge next to the press. Heat a piece to welding pull it out weld, heat
the
> next area and then slide it back and forth leaving it in the forge.
>
> He poured castible refractory in the bottom but left a hole for flux and
> gunk to drip out then lined the side walls with Kaowool. He stuck a piece
> of wool on the top and placed a lose piece of steel on top of that. He
said
> that was the insurance so when you open the gas then light the forge and
it
> goes boom it only rains kaowoll and not steel shrapnel.
>
> A couple of other things he preached is mount the blower outlet pipe so it
> slides on and off the outer shell of the forge. He welded a 1/2" round
rod
> bent into a 90 on the outer shell then had a collar that slipped on this
to
> hold the blower in place. The advantage to this is you can have one
blower
> set up and 50 different sized forges. Another thing he said was to have a
> needle valve for gas adjustment. According to him a ball valve is too
gross
> of adjustment.
>
> UMBA does have a DVD of this but it is not listed on the web site yet. I
> keep saying as soon as I finish the next DVD I will send in the new list
but
> then I keep signing up for class. I have a 3 day with Kirsten Sikes on
> chasing and reposse. Just finished a 3 day with her husband Bill Fiorini
on
> Japanese stamping tech. The new list now goes to RD151 and Salt7
>
> Roger R Degner
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com