[TheForge] standard materials on hand

Peter Fels & Phoebe Palmer artgawk at thegrid.net
Sun Jun 14 22:33:19 EDT 2009


Sounds good to me for both parties.
What sort of fish?  pf

Bob Ehrenberger wrote:
> He gave me the pins as a thank you for letting him fish in my pond, so it's 
> a fair exchange, fish for scrap iron.
> 
> Robert Ehrenberger
> Shelbyville, Mo.
> eforge at centurytel.net
> 
> 
> ----- Original Message ----- 
> From: "Peter Fels & Phoebe Palmer" <artgawk at thegrid.net>
> To: "Bob Ehrenberger" <eforge at centurytel.net>; "Blacksmithing List Sponsored 
> by ABANA" <theforge at mailman.qth.net>
> Sent: Sunday, June 14, 2009 2:49 PM
> Subject: Re: [TheForge] standard materials on hand
> 
> 
> Just different uses Bob. Quite possibly 4140. Be nice to that
> friend..there are some wonderful Cat parts for a guy inclined to make
> his own tools.
> I got a giant, cracked CV joint, for example, that has become 3 forming
> stakes already and there's still some of it left.
> 
> Bob Ehrenberger wrote:
>> 2 1/2 shaft is a great find,  I have almost no really large stuff to work
>> with.  A friend that works for a CAT repair shop gave me some large king
>> pins, but they all have a lube hole down the center, kind of limits their
>> usefulness.
>>
>> Robert Ehrenberger
>> Shelbyville, Mo.
>> eforge at centurytel.net
>> 573-633-2010
>>
>> ----- Original Message ----- 
>> From: "Jeff & Leslie" <barkingcrow at comcast.net>
>> To: "Bob Ehrenberger" <eforge at centurytel.net>; "Blacksmithing List 
>> Sponsored
>> by ABANA" <theforge at mailman.qth.net>
>> Sent: Sunday, June 14, 2009 10:42 AM
>> Subject: Re: [TheForge] standard materials on hand
>>
>>
>> Keep checking those trash piles!  Today between two old washing machines,
>> and under a crappy folding chair I found a 29" piece of 2 1/2" shaft!  A
>> pretty good find.  A small anvil is what it will be.
>>
>> Smiling Jeff in brutally hot and humid Tallahassee
>>
>>
>>
>> --------------------------------------------------------------------------------
>>
>>
>>
>> No virus found in this incoming message.
>> Checked by AVG - www.avg.com
>> Version: 8.5.339 / Virus Database: 270.12.68/2175 - Release Date: 06/14/09
>> 05:53:00
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> 
> 
> 
> --------------------------------------------------------------------------------
> 
> 
> 
> No virus found in this incoming message.
> Checked by AVG - www.avg.com
> Version: 8.5.339 / Virus Database: 270.12.68/2175 - Release Date: 06/14/09 
> 05:53:00
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 


More information about the TheForge mailing list