I do not know about historically, but the best way is to get some
spring steel and harden and drawn-back.  My uncle used to do this for
small parts with a MAPP gas/Oxy torch.

David Childress
Rocky Forge Blacksmith Guild

On 7/31/09, David E. Smucker <davesmucker at hotmail.com> wrote:
> Dave,  You need to case harden the spring part.  This what was done
> historically on many very old firearms.
>
> Do a google search under  < case hardening gun parts > there is a lot of
> information including so video.
>
> Dave
>
> --------------------------------------------------
> From: "Dave Kammer" <tinman36 at yahoo.com>
> Sent: Friday, July 31, 2009 10:31 AM
> To: <theforge at mailman.qth.net>
> Subject: [TheForge] hardening steel
>
>> I was looking for some advice on how to harden a small piece of steel. I
>> have an old shotgun with a broken hammer spring, Parts for this old gun
>> are unavailable, so I was able to make a duplicate but it is too soft of
>> steel. It needs to spring back and forth. The piece I made just bends when
>>
>> put under pressure. Can some sort of heat treatment or hardening make it
>> become more spring-like?
>>
>>
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>


More information about the TheForge mailing list