I mix in a little lime to take out water.?
----- Original Message -----
From: "Peter Fels & Phoebe Palmer" <artgawk at thegrid.net>
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, July 16, 2009 1:31 PM
Subject: Re: [TheForge] Vermiculite
> In defense of ash...if one selectively chooses the fine, fluffy, white
> ash from wood burning..it seems more insulative than the rest.
> I bet including some fin ground charcoal wouldn't hurt either.
>
> Jay Hayes wrote:
>> I got some vermiculite at Lowes and Southern States last year. It is a
>> seasonal item, but they might still have some or can get it.
>>
>> Jay
>>
>> Bob Ehrenberger wrote:
>>> Hi Guys,
>>>
>>> I have a barrel of vermiculite that I use to anneal tools and knives.
>>> Over
>>> the years the vermiculite has gotten compacted and is only about half
>>> full
>>> now. I wanted to get some more to top it off and have discovered that
>>> it is
>>> no longer available at most farm & home stores like it used to be.
>>>
>>> It seems that most of the gardening departments have switched to perlite
>>> instead of vermiculite. Have any of you used perlite for annealing?
>>> Does
>>> it work as well and vermiculite? Would it hurt to mix it with the
>>> vermiculite that I have left?
>>>
>>> Robert Ehrenberger
>>> Shelbyville, Mo.
>>> eforge at centurytel.net
>>>
>>>
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>>
>>> TheForge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>>
>>> This list hosted by: http://www.qsl.net
>>> Please help support this email list: http://www.qsl.net/donate.html
>>> ------------------------------------------------------------------------
>>>
>>>
>>> No virus found in this incoming message.
>>> Checked by AVG - www.avg.com
>>> Version: 8.5.375 / Virus Database: 270.13.15/2239 - Release Date:
>>> 07/15/09 06:07:00
>>>
>>>
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list