Hello
As described that means that the bottom is the heavier and that the top
is the lighter, then why would you remove more from the lighter side?
lynn
>The shade tree approach would be to suspend the shafted assembly
between
>2 sharp, hardened points in the centering holes on the shaft ends, in a
>lathe. Then give it some whirls and mark the bottom points when it
>stops moving. Shave off metal opposite the marks and repeat till crazy
>and the marks distribute randomly.
>But i doubt that'll get you to 10,000 RPM.