[TheForge] cutting stainless (a little OT)

Andy Gladish gladish at cablerocket.com
Fri Jul 10 15:07:21 EDT 2009


Thanks!
I bet it's a speed issue, I had the sawzall speed backed way off for  
cutting a36, probably way too fast still for stainless.
Blades get eaten quickest on that, then portaband (which was running on  
faster speed setting), horizontal saw seems ok and wouldn't you know it?  
is the slowest of the bunch.

Andy G.

On Fri, 10 Jul 2009 11:58:46 -0700, ries <ries at riesniemi.com> wrote:

> how fast you going?
> Slower is probably better.
> tooth spacing?
> 3 teeth in the metal is the optimum- obviously, thats not always
> practical, but for 1/8" to about 3/4" thick material, I find the 10-14
> variable pitch lennox blades work pretty well. Thinner than 1/8", you
> need a finer blade, up past 1" or so, a coarser one.
> Are you freehand cutting, or using a horizontal band saw?
> freehand will eat saw blades the fastest, as its much easier to jam it
> in and break a tooth.
> With bi-metal blades, once one tooth goes, the rest start ripping out
> in short order.
> I find the Lennox blades last a month or so of cutting stainless, not
> all day, but a lot of cuts.
> 304 will not vary much in hardness, from annealed to fully hard, so
> its probably not a hardness/temper issue.
> I use cool tool for a lube, just cause it works on most everything- I
> use it for drilling, milling, turning, sawing, and sometimes even
> tapping, and it is relatively non-toxic.
> But cutting oil of most any type should help.
>
> ries
>
>
> On Jul 10, 2009, at 11:14 AM, Andy Gladish wrote:
>
> Yikes!
> This stainless bar is eating my saw blades!
> I only use Lenox bi metal, assumed that it would be tough enough...any
> suggestions?
>
> Thanks!
> Andy G.
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> Ries Niemi
> Industrial Artist
> http://www.riesniemi.com/
>
>
>
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html



-- 
Andy Gladish, Metal Work
Element Forge
www.ElementFe.com
Online Store at: ElementFe.Etsy.com
Email:  andy at elementfe.com
Portfolio @  elementfe.carbonmade.com
Work blog @ elementfe.blogspot.com

Benjamin Franklin said : 'So convenient a thing it is to be a reasonable  
creature, since it enables one to find or make a reason for everything one  
has a mind to do.'


More information about the TheForge mailing list