I would check the mounting all around the glass to make sure one side isn't
screwed. If not grind or otherwise remove welds or rivets, make a template
from the glass and find a fire place supply to send the template out to get
you a piece of glass. If there is no gasket around the glass this may be
why it broke
When reattaching use screws if possible
Larry Brown
At 09:04 AM 1/30/2009 -0500, you wrote:
>My son says one of the glass pieces on his fireplace doors broke. This is
>a commercial unit that was in the house when he bought it. I have not
>looked at it yet but he says the frame is either welded or riveted and
>that there is no way to remove the glass. He also said the glass was in
>two pieces horizontally and just butted together.
>
>I know .... I know ... but I don't have time for another project right now.
>
>Have any of you looked at similar units and is there a way to repair
>this? Or do I have yet another project?
>
>Thanks,
>Walt
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
More information about the TheForge
mailing list