[TheForge] Green concrete
Clyde
clyde at fibernetcc.com
Mon Jan 19 08:27:49 EST 2009
I think that the green concrete information wanted is the concrete with the
fly ash. Here is one of Google's many references to it:
DENVER -- The next time you are in downtown Denver, take a look around. All
of the concrete you see plays a large role in our carbon footprint.
What you may not know is that Denver is the first city to include the impact
of making building materials into its greenhouse gas inventory.
Unlike other cities that only measure common air pollutants such as car
emissions and factory emissions, Denver counts the effect of producing its
building materials as well.
This has led to unique climate action policies in our city, including the
use of a "green" concrete.
Dr. Anu Ramaswami and her colleagues in the University of Colorado -Denver's
environmental engineering department hope the city will use the high
performance green concrete in upcoming projects.
"What's new for us is to show that this material can be used in all
applications, in all cities," said Ramaswami.
Fly ash, a reusable byproduct from power plants that is often thrown away,
is now being used in making green concrete, to replace some of the cement.
Less cement means a healthier environment.
In fact, UCD's recent project on Urban Sustainable Infrastructure reveals
that, by replacing convention concrete with 20 percent fly ash concrete, the
city can save carbon emissions equivalent to that of removing more than
10,000 cars from Denver roads each year.
The green concrete is tested for strength and durability to be certain it
can endure Colorado's variable climate. In all areas, it has performed
better than traditional materials.
"It is more green, more economical, more durable, and has higher strength,"
said Stephan Durham, an assistant professor at UCD.
Green concrete will also save the city money.
"Something that we would otherwise put in the landfill we are reusing in our
construction, which means we don't have to buy and transport new, raw
materials," said Michele Weingarden, the director of Green Print Denver. "We
are going to find everywhere possible to put green concrete."
Contractors are pouring green concrete at an area that will extend 40th
Avenue north of Stapleton.
"You might be seeing curb and gutter repair using green concrete as well as
some street repaving projects," said Weingarden.
And that will put Denver in the national spotlight, according to UCD
scientists.
"Other cities could use Denver as a stepping stone, a good stepping stone
for what other cities can do to be more environmental," Durham said.
Here are some links that you can visit for more information on green
concrete in Denver:
. www.greenprintdenver.org <http://www.greenprintdenver.org/>
. www.envirocore.us <http://www.envirocore.us/>
For more information on UCD's graduate research program, go to
cudenver.edu/IGERT <http://cudenver.edu/IGERT/> .
-------------- next part --------------
An HTML attachment was scrubbed...
URL: http://mailman.qth.net/pipermail/theforge/attachments/20090119/7c40b700/attachment.html
More information about the TheForge
mailing list