My only comment is that you can drive a nail thru a copper line and you
can't usually hurt a steel pipe. But copper is a lot easier to use than
steel.
I plumbed my shop air system w/ 3/4" sch 40 pvc, about 250' of it so
far. It has far more limitations than copper but is even cheaper and
easier.
I just turn the valve at my compressor each night, isolating the
compressor in case the line breaks or I have a leak.
James
> 6. Shop Air using Copper (bistline at md.metrocast.net)
>
>
> Subject:
> [TheForge] Shop Air using Copper
> From:
> bistline at md.metrocast.net
> Date:
> Tue, 13 Jan 2009 09:21:31 -0500 (EST)
> To:
> theforge at mailman.qth.net
>
> To:
> theforge at mailman.qth.net
>
>
> Trying to get hard air lines set up in my shop. Went to lowes to buy
> "iron" pipe and noticed its made in Korea brand name Tuna. At many levels
> that just bothers me. I turn around to see copper made in the USA. Believe
> it or not the type L 3/4 copper is $1.25 a 10ft stick cheaper than the
> "iron". I notice type m copper that is $5 cheaper yet. The type L has a
> slightly thicker wall thickness. I know that the standard for air lines is
> "iron pipe" however a little web searching has revealed copper is commonly
> used. *_Any inputs on copper for air lines_?*
>
>
>
>