[TheForge] Belt grinder lube..

Jerry Frost akfrosty at mtaonline.net
Fri Jan 9 16:31:51 EST 2009


I apply a little parafin wax to the back of the belt on 
mine, it makes it run easier.

Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks

Meadow Lakes, AK.


From: "Todd Rich" <torin at panix.com>


>
> I was looking up getting some cutting wax for my 
> bandsaw on MSC and I
> notice that they have a wax type lube for 
> grinders/sanders.  I've always
> used my belt grinder dry before.  Is this something I 
> should consider
> getting?  Will it help for knife grinding on pattern 
> welded material?
>  Todd
>
> 


More information about the TheForge mailing list