[TheForge] Wooden Hammer Handles

Peter Hirst saltydog335 at aol.com
Wed Jan 7 22:31:52 EST 2009


Like a baseball bat:  the flat grain on the sides, the vertical or narrow 
grain with the striking edge.
----- Original Message ----- 
From: "Lynn and Susan Lang" <langfarm at together.net>
To: <theforge at mailman.qth.net>
Sent: Wednesday, January 07, 2009 9:59 PM
Subject: [TheForge] Wooden Hammer Handles


> Hello
>
>
> I am in the process of splitting out new hickory handles for my hammers.
> My question is: should the grain run parallel to the swing arch or
> should it run perpendicular?
>
>
>
> Thank you
> lynn
>