[TheForge] Wooden Hammer Handles

dan tull dantull at numail.org
Wed Jan 7 22:11:12 EST 2009


Parallel.
A knot in that plane would not be stressed as other way.


----- Original Message ----- 
From: "Lynn and Susan Lang" <langfarm at together.net>
To: <theforge at mailman.qth.net>
Sent: Wednesday, January 07, 2009 9:59 PM
Subject: [TheForge] Wooden Hammer Handles


> Hello
> 
> 
> I am in the process of splitting out new hickory handles for my hammers.
> My question is: should the grain run parallel to the swing arch or
> should it run perpendicular? 
>          
> 
> 
> Thank you
> lynn
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
>


More information about the TheForge mailing list