Not well by my standards. If it *requires* maintenance, then it is not
a good outdoor finish.
Wayne Ackman wrote:
> I have used a rust finish several times. -- sandblast, wire brush, etc,
> then rusted and waxed. Finally a clear coat of lacquer. How well would
> this finish hold up outside?
--
-Andy Vida