Peter;
Does that mean we are drinking those copper oxides?..peter f
Peter Hirst wrote:
> What's eating your copper is acidic water: can be treated with a filter
> tank. A little pricey, but sometjhimes you can pick them up cheap to
> free from people switching over to municipal water from a well. except
> for slight acid (my copper is just beginning to develop pinholes after
> 35 years) my well water is the best, and i wouldn't trade it for
> anything. So I picked up a filter and will replace the copper piece by
> piece with good solid used stuff as I acquire it. It will last a
> lifetime with the filter, and since I have so much exposed plumbing in
> the house, it is well worth it to me.
>
>
> ----- Original Message ----- From: "David E. Smucker"
> <davesmucker at hotmail.com>
> To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Friday, January 02, 2009 7:19 PM
> Subject: Re: [TheForge] OT frozen pipes
>
>
>> Andy,
>>
>> How does copper work in your area? I was always a fan of copper until
>> we moved here to Brasstown, NC. With most of the well water in this
>> area, it eats copper -- so any of the plastics are better. Dad had
>> the same problem when they moved to Boulder, CO. Just check around
>> before you go to copper. The well drillers here are the ones that told
>> me to stay away from copper -- most of the hardware stores here don't
>> even carry it any more. (and I had lots of copper fittings on hand
>> when I built this house.)
>>
>> Dave
>>
>> --------------------------------------------------
>> From: "Andrew Vida" <osan at netlabs.net>
>> Sent: Friday, January 02, 2009 11:21 AM
>> To: "Bob Ehrenberger" <eforge at centurytel.net>; "Blacksmithing List
>> Sponsored by ABANA" <theforge at mailman.qth.net>
>> Subject: Re: [TheForge] OT frozen pipes
>>
>>> Sharkbite fittings are, as you say, pricey, but they really do work.
>>> My plan for this house is to replace all the lousy PVC lines with
>>> copper and sharkbite fittings. Those fittings will also work with
>>> PVC and any other rigid or semi-rigid tubing. Very ingeniously
>>> contrived, BTW.
>>>
>>> Bob Ehrenberger wrote:
>>>> The Monday before Christmas we had the temps drop below zero with
>>>> high winds out of the West. As a result, the pipes that run to our
>>>> laundry froze and burst. That section of the house is just a crawl
>>>> space, so instead of opening up the hatch to gain access which would
>>>> have really flooded the space with cold air, I decided to disconnect
>>>> and cap that section at the source. I got the Hot line capped ok,
>>>> but the shut off valve did not stop the flow completly and let a
>>>> steady drip through to the cold line. Because of the dampness, I
>>>> couldn't get the joint to take solder, so I decided to use a
>>>> compression fitting. At the local farm store they didn't have any
>>>> compression fittings, but they had something called SharkBite. It
>>>> was a bit pricey but what option did I have? So I got it. To my
>>>> amazment, it worked as advertised, just clean the end and slide the
>>>> fitting on and you are done. So if you have to make an emergency
>>>> repair, the SharkBite connectors are a good choice.
>>>>
>>>> Robert Ehrenberger
>>>> Shelbyville, Mo.
>>>> eforge at centurytel.net
>>>>
>>>>
>>>> _______________________________________________
>>>> Manage membership or unsubscribe at:
>>>> http://mailman.qth.net/mailman/listinfo/theforge
>>>> theforge mail list group photo site is
>>>> http://www.photoaccess.com
>>>> Login: blacksmithblacksmith at hotmail.com
>>>> password: anvil
>>>> ___________
>>>>
>>>>
>>>
>>> --
>>>
>>> -Andy Vida
>>>
>>> Proof Technologies Inc.
>>> IV&V
>>> Project and Program Management
>>> (304) 466-0789
>>> /\
>>> __ / \ __
>>> \ \/ /\ \/ /
>>> \ \/ \ \/
>>> /\_\__/\ \
>>> / ____/ /_ \
>>> /_/ \ / \_\
>>> \/
>>>
>>>
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> password: anvil
>>> ___________
>>>
>>>
>>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list