[TheForge] Glass question
Bruce Freeman
freemab222 at gmail.com
Wed Feb 25 13:38:42 EST 2009
Larry,
I expect the stuff will shatter the moment you touch a grinder to it.
This is a job for professionals.
On Wed, Feb 25, 2009 at 8:56 AM, Andrew Vida <osan at netlabs.net> wrote:
> I'm not a big glass expert, but I would think that you'll be OK.
> Tempered glass is pretty tough stuff.
>
> Larry Brown wrote:
>
>> The question is other than removing the unwanted glass will this promote
>> cracking since the glass is tempered?
>> Larry Brown
>
> --
>
> -Andy Vida
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Bruce
NJ
The total lack of evidence is the surest sign that the conspiracy is working.
More information about the TheForge
mailing list