Does that mean it'll melt at higher temperatures?
Chris Caswell wrote:
> At the lighting shop I work at, we use a commercial heat gun to soften
> the mica, then bend it over a form.
>
> Chris Caswell
> Caswell Wood & Iron
>
>
>
> Michael Horgan wrote:
>> What sort of manipulation did you have in mind, Mark? Mostly you can
>> cut it, split it, bend it slightly. I got a book of mica once,(long
>> ago, pre web, sigh), and split off sheets to use in a lantern. To
>> bend it you would need to frame it to keep it under tension.
>> For a little more info take a look at http://micasales.com/
>>
>> Michael
>>
>> At 06:25 AM 12/6/2009, you wrote:
>>
>>> My last post got one serious posting and then derailed, so I'll ask
>>> again. Does anyone have any good resourses for the manipulation of
>>> mica sheet? I saw a lot of it at the last Northwest Blacksmith assoc
>>> Conference, but there were no lectures.
>>>
>>> M
>>> ______________________________________________________________
>>> TheForge mailing list
>>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>>> Help: http://mailman.qth.net/mmfaq.htm
>>> Post: mailto:TheForge at mailman.qth.net
>>>
>>> TheForge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> Password: anvil
>>>
>>> This list hosted by: http://www.qsl.net
>>> Please help support this email list: http://www.qsl.net/donate.html
>>>
>> Michael D. Horgan , lughaid at earthlink.net
>> posting from
>> A BRAZEN FORGERY
>> Blacksmithing and Metalwork
>> Claremont, Ca.
>>
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
>>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list