Some of the mica sheets were used flat, but others were either curved  
for a sconce or even twisted for a light fixture (rectanglse 6"x1.5'  
twisted on a single central axis). The twisted mica was not framed in  
any visible way. It looked as if it had been twisted and then held the  
shape unassisted.