[TheForge] Sealing a fireplace screen

Larry Brown lp.brown at verizon.net
Thu Aug 13 04:52:01 EDT 2009


Thanks


At 10:36 PM 8/12/2009 -0400, you wrote:
>French polish (shellac in alcohol) alternating or mixed with boiled linseed
>oil.
>
>
>----- Original Message -----
>From: "Larry Brown" <lp.brown at verizon.net>
>To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
>Sent: Wednesday, August 12, 2009 10:29 PM
>Subject: Re: [TheForge] Sealing a fireplace screen
>
>
> > More info?
> > L Brown
> >
> > At 09:38 PM 8/12/2009 -0400, you wrote:
> >>French oil finish.



More information about the TheForge mailing list