Option 1; Figure out why it was messed up to begin with, stress, abuse. If 
the dump action attaches there, its a lot of stress. You could change the 
whole   piece if you are getting paid. I would add supports inside the web 
(Fish plates) if possible in that area to prevent future breakage.

Option 2; If you are unlucky enough to be doing this with out proper 
compensation. Figure out why it was messed up to begin with, stress, abuse. 
Cut out broken weld, re weld, Fishplate with heavy stock inside the webs 
and if there is clearance top and bottom of beam, Several feet long, I 
would try for at least 18" each side if there is clearance, more if 
possible. Cut corners of fishplates off. Only weld ends in center of beam 
just to hold down and space welds along top and bottom to anchor over 
repair. I would try not to weld the whole length but weld several inches, 
skip several, weld, etc

I was shown by a tank welder that acetone helps get a good mig weld when 
used for cleaning instead of an acid.
Warning; Acteone fumes can Go BOOM if not ventilated, so I didn't tell you 
this. Dump body has open air, just don't put the can between your feet

Hope this answers your question or helps solve your problem. Figure out the 
initial problem first, it may save you time if you can see why it broke

L Brown


At 06:54 PM 8/12/2009 -0400, you wrote:
>I welded an aluminum dump truck dump body frame rail together since a
>4 foot section had to be replaced at the pivot end. I replaced the 6
>inch I beam with a new one and I welded it together. The owner has
>contacted me that the weld broke. I fixed it and gave it back. He now
>said it did it again. It is breaking from the top of the beam down.
>
>I made straight cuts and there was about a 3/8 inch between the old
>one and the new piece. I mig welded the outside after I cleaned the
>joint with a brand new stainless steel wire wheel and then aluminum
>cleaner, muradic acid. I welded it at proper settings and helium gas.
>I even cross stitched weld over the vertical weld to improve strength.
>I am using 4043 3/64 wire
>
>After it broke the first time, I asked other welders what I did wrong,
>they don't know. I am loosing my mind trying to figure it what I am
>doing wrong. I do not have a welder heavy enough to put out 250 amps
>to tig weld it but I do have a 302 trailblazer that I could run 225
>amps to tig it. I don't know what to do besides replacing the entire
>beam and eliminate the weld.
>
>--
>Sent from my mobile device
>______________________________________________________________
>TheForge mailing list
>Home: http://mailman.qth.net/mailman/listinfo/theforge
>Help: http://mailman.qth.net/mmfaq.htm
>Post: mailto:TheForge at mailman.qth.net
>
>TheForge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>Password: anvil
>
>This list hosted by: http://www.qsl.net
>Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list