All i know from playing with it is that Nickel kicks up the forging 
temperature of an alloy.

Jerry Frost wrote:
> An acquaintance asked me the following question but I don't have any direct 
> experience. How about you guys?
> 
> Frosty
> -------------------------
> If it ain't forged
> It ain't real
> wrought iron is
> The Frostworks
> 
> 
>> Frosty,
>>
>> I am wondering if you know anyone who could advise me on forging nickel
>> alloys. All I can find is related to damascus and I want to know about
>> forging larger peices (1" plus) of nickel.
>>
>> Thanks,
>>
>> Magnus 
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 


More information about the TheForge mailing list