Quit trying to TIG high zinc alloys :-)
Unless it is silicon bronze or gold trying to TIG yellow metal sucks.
Some of the phosphor bronzes are so so but brass with enough zinc to
be yellow is just not suitable for TIG
James Binnion
jbin at well.com
On Aug 2, 2009, at 3:40 PM, Peter Fels & Phoebe Palmer wrote:
> It's the John Cage school of BS communication?
> I'm still having trouble TIGging brass...Keeps flashing and fuming
> zinc
> instead of puddling. Any suggestions? pf