[TheForge] vise repair

Allen Ortery bluestoneforge at gmail.com
Fri Apr 24 09:55:34 EDT 2009


We just repaired a vise this way, female threads where milled on the
original. worked very well and if done right you can't tell with out
looking very close

--
Allen Ortery
bluestoneforge at gmail.com
309-368-7967