[TheForge] Forging a post vice
Andrew Vida
osan at netlabs.net
Wed Apr 22 10:12:11 EDT 2009
Your crazy friend better be very well equipped, not only to hand 100#+/-
of very hot iron, but to protect himself from the radiant heat. Largest
piece of iron I have ever had at welding heat was maybe 20 or 30 pounds
with perhaps 10 of those at bright yellow. The amount of radiant energy
such a mass throws off is nothing to be casual about. It will burn you
seriously from feet away.
I would also say that unless he has experience with the industrial
forging of masses that large, he is going to have a hard time. It isn't
like hammering a taper on a piece of 3/4 square. It isn't ANYTHING like it.
Ron Childers wrote:
> Thankx for your help. That is the one, but my crazy friend will probably
> want to scale it up to 6" jaws ...
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Larry Brown
> Sent: Wednesday, April 22, 2009 5:12 AM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] Forging a post vice
>
> This should do it;
> http://www.lightningforge.com/upload61/vise.htm
>
>
> At 08:54 AM 4/22/2009 +0100, you wrote:
>> Well I'm interested even if no-one else is!
>>
>> Rich M.
>>
>> Richard Maynard - Artist Blacksmith
>> The Forge, Much Hadham, Hertfordshire SG10 6BS
>>
>> The Forge Experience - be a blacksmith for a day!
>> http://www.muchhadhamforge.co.uk/experience.pdf
>>
>> rich at muchhadhamforge.co.uk
>> www.muchhadhamforge.co.uk
>>
>>
>> -----Original Message-----
>> From: theforge-bounces at mailman.qth.net
>> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Larry Brown
>> Sent: 22 April 2009 02:01
>> To: Blacksmithing List Sponsored by ABANA
>> Subject: Re: [TheForge] Forging a post vice
>>
>>
>>
>>
>> I was just inadvertently send the plans by a Forge member and I realized I
>> published them In the NJBA newsletter (A long time ago, volume 6 and I'm up
>> to 14 now). If there is any interest I'll post them and send the URL Larry
>> Brown
>>
>>
>> At 01:37 PM 4/21/2009 -0700, you wrote:
>>> There was a series of articles in the Anvil's Ring on restoring a
>>> postvise a while back.
>>>
>>> Ben Barrett wrote:
>>>> Hurm, I seem to remember something like that too, but I also cannot
>>> find it.
>>>> This might be a good ref though:
>>>> http://www.anvilfire.com/FAQs/vises.htm
>>>>
>>>> Ben
>>>>
>>>>
>>>> On Tue, Apr 21, 2009 at 5:00 AM, Ron Childers <munlaw2 at hcsmail.com>
>>>> wrote:
>>>>
>>>>> A friend of mine thinks he wants to forge a post vice. There was an
>>> article
>>>>> in a publication or maybe on the internet about making a post vice
>>>>> that I skimmed through it but don't remember the source. Does
>>>>> anyone know where I might have seen that article?
>>>>>
>>>>> Thanx,
>>>>>
>>>>> Ron C
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
>
>
>
>
> ****************************************************************************
> ********
> This footnote confirms that this email message has been scanned by
> PineApp Mail-SeCure for the presence of malicious code, vandals & computer
> viruses.
> ****************************************************************************
> ********
>
>
>
>
>
>
>
>
>
> ************************************************************************************
> This footnote confirms that this email message has been scanned by
> PineApp Mail-SeCure for the presence of malicious code, vandals & computer viruses.
> ************************************************************************************
>
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
-Andy Vida
/\
__ / \ __
\ \/ /\ \/ / Proof Technologies Inc.
\ \/ \ \/ IV&V, Project and Program Management
/\_\__/\ \ Coming soon: parts for Star Reloaders
/ ____/ /_ \ (304) 466-0789
/_/ \ / \_\ osan at netlabs.net
\/
More information about the TheForge
mailing list