[TheForge] Re: yurts, spelter sockets
Mike Spencer
mspencer at tallships.ca
Tue Apr 21 19:02:03 EDT 2009
> ...the spelter process is roughly illustrated at our Sahale bridge
> site www.sahale.com<http://www.sahale.com/> under the Meriwether
> bridges.
> [snip]
> Two things are very important in the process. Number one is the
> proper 'brooming' of the strand. This is a manual process where you
> carefully 'unwind' the lay of the cable and stretch it out into a
> cone shape. This helps the zinc to grab each strand as much as
> possible. Secondly is the temp. of the pour. We shoot for 1080F
> which is hot enough to withstand being in the ladle for awhile as the
> pour progresses. The cable or strand is stripped with muriatic and
> force-dried with a weed-burner for a little bit of preheat. Be
> careful though because too much heat will anneal th e wires. Any
> color in them and you're too hot.
Thanks for the details, Steve. Seeing the size of the cable you're
working with puts a whole 'nother light on the process. If I have to
do something with 3/4" I feel like I'm getting into the Big-Time. :-)
- Mike
--
Michael Spencer Nova Scotia, Canada .~.
/V\
mspencer at tallships.ca /( )\
http://home.tallships.ca/mspencer/ ^^-^^
More information about the TheForge