[TheForge] Question on RR steel.

Ron Childers munlaw2 at hcsmail.com
Mon Apr 20 11:28:17 EDT 2009


Jeff, 

I think you are talking about the metal used to thermit weld the tracks-
notice they are found close to the red 7 white rubble used as a "dam" to
concentrate the weld. The weld is then ground to the configuration of the
rest of the track. My guess is it is close to the same material as the
track. I know a fellow who forged a piece on the power hammer and he said
when etched, it had a mottled appearance. 

Maybe someone with railroad experience can give us a more specific answer;
that's just my swag.

Ron C

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Jeff & Leslie
Sent: Monday, April 20, 2009 11:08 AM
To: Blacksmithing List Sponsored by ABANA
Subject: [TheForge] Question on RR steel.

Not too long ago someone was explaining the different pieces found along RR 
tracks.  I occasionally find pieces of round stock usually around 8 - 10" 
long and fonged to a square taper on one end.  Taper is about 4" long.  The 
rod is 1 3/4" in diameter.  I'd like to know what they are and what they're 
made of.  My spark testing skills tell me that they're probably metal.

Thanks,  Jeff in Tallahassee where it should get down to about 50 tonight 
for probably the last time till next fall 

______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html



 
 




 
 
************************************************************************************
This footnote confirms that this email message has been scanned by
PineApp Mail-SeCure for the presence of malicious code, vandals & computer viruses.
************************************************************************************





More information about the TheForge mailing list