> Hey Steve,
> My Yurt Smithy has been thru 3 hurricanes including 
> being at ground Zero in
> Katrina.
> The uprights are 5" drill stem ( 4141 -5/8" wall 
> pipe) and strung together
> with 3/4" double improved plow steel wire rope. The 
> drill stem is anchored
> in 3" of reinforced concrete 6' deep.
> Have had (4) 95' pine trees blown down on it, with 
> minimal roof damage.
> The trunks, when they hit the wire rope, stop dead
> Chuck