[TheForge] Blacksmithing, treadle hammer

Peter Fels & Phoebe Palmer artgawk at thegrid.net
Fri Apr 3 15:27:07 EDT 2009


An additional point on welded TH anvils...orient the steel vertically, 
horizontal joints or laps that aren't 100% penetration welded absorb energy.

Ron Childers wrote:
> 
>  
> 2 points:
> Make sure that the anvil is solid steel.  You need that mass under the
> hammer.  there were some designs out there that had hollow anvils, or anvils
> filled with concrete or concrete and scrap metal. 
> Make sure that both the hammer and anvil have hardy holes for tooling. IIRCC
> at one time the Jere Kirkpatric's design did not have a hardy hole in the
> hammer part.
> 
> D-ski 
> Westminster, MD     
> The lyf so short, the craft so long to lerne.
> 
> 
> You are correct on the solid steel; the heavier the better, but the anvil
> can be welded up from slabs of steel, ie 3 pcs of 2"x6" or even a 3' pc of
> rr track with additional pcs of steel welded to it to if the budget is tight
> and you don't mind the junk yard look. The anvil doesn't care as long as the
> solid weight = a 3' piece of 5" round.
> 
> Ron C
> 
> 
> 
> 
> 
>  
>  
> ************************************************************************************
> This footnote confirms that this email message has been scanned by
> PineApp Mail-SeCure for the presence of malicious code, vandals & computer viruses.
> ************************************************************************************
> 
> 
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 


More information about the TheForge mailing list